SAMPATH, Sridhar, Philipp MAYDANNIK, Tatiana IVANOVA, Marina SHESTAKOVA, Tomáš HOMOLA, Anton BRYUKVIN, Mika SILLANPÄÄ, Rameshbabu NAGUMOTHU and Viswanathan ALAGAN. Efficient solar photocatalytic activity of TiO2 coated nano-porous silicon by atomic layer deposition. Superlattices and Microstructures. 2016, vol. 97, september, p. 155-166. ISSN 0749-6036. Available from: https://dx.doi.org/10.1016/j.spmi.2016.06.004.
Other formats:   BibTeX LaTeX RIS
Basic information
Original name Efficient solar photocatalytic activity of TiO2 coated nano-porous silicon by atomic layer deposition
Authors SAMPATH, Sridhar (356 India, guarantor), Philipp MAYDANNIK (643 Russian Federation), Tatiana IVANOVA (643 Russian Federation), Marina SHESTAKOVA (643 Russian Federation), Tomáš HOMOLA (703 Slovakia, belonging to the institution), Anton BRYUKVIN (643 Russian Federation), Mika SILLANPÄÄ (246 Finland), Rameshbabu NAGUMOTHU (356 India) and Viswanathan ALAGAN (356 India).
Edition Superlattices and Microstructures, 2016, 0749-6036.
Other information
Original language English
Type of outcome Article in a journal
Field of Study 10305 Fluids and plasma physics
Country of publisher United Kingdom of Great Britain and Northern Ireland
Confidentiality degree is not subject to a state or trade secret
WWW http://www.sciencedirect.com/science/article/pii/S0749603616302567
Impact factor Impact factor: 2.123
RIV identification code RIV/00216224:14310/16:00090205
Organization unit Faculty of Science
Doi http://dx.doi.org/10.1016/j.spmi.2016.06.004
UT WoS 000385319200017
Keywords in English Porous silicon;TiO2;Stain etching;ALD;Layer by layer solar absorption
Tags AKR, rivok
Changed by Changed by: Ing. Andrea Mikešková, učo 137293. Changed: 5/4/2017 11:31.
Abstract
In the present study, TiO2 coated nano-porous silicon (TiO2/PS) was prepared by atomic layer deposition (ALD) whereas porous silicon was prepared by stain etching method for efficient solar photocatalytic activity. TiO2/PS was characterized by FESEM, AFM, XRD, XPS and DRS UV–vis spectrophotometer. Absorbance spectrum revealed that TiO2/PS absorbs complete solar light with wave length range of 300 nm–800 nm and most importantly, it absorbs stronger visible light than UV light.
Links
ED2.1.00/03.0086, research and development projectName: Regionální VaV centrum pro nízkonákladové plazmové a nanotechnologické povrchové úpravy
LO1411, research and development projectName: Rozvoj centra pro nízkonákladové plazmové a nanotechnologické povrchové úpravy (Acronym: CEPLANT plus)
Investor: Ministry of Education, Youth and Sports of the CR
PrintDisplayed: 3/10/2024 09:21