Detailed Information on Publication Record
2016
On the study of the mechanical properties of Mo-B-C coatings
ZÁBRANSKÝ, Lukáš, Vilma BURŠÍKOVÁ, Pavel SOUČEK, Petr VAŠINA, Jiří BURŠÍK et. al.Basic information
Original name
On the study of the mechanical properties of Mo-B-C coatings
Authors
ZÁBRANSKÝ, Lukáš (203 Czech Republic, belonging to the institution), Vilma BURŠÍKOVÁ (203 Czech Republic, guarantor, belonging to the institution), Pavel SOUČEK (203 Czech Republic, belonging to the institution), Petr VAŠINA (203 Czech Republic, belonging to the institution) and Jiří BURŠÍK (203 Czech Republic)
Edition
The European Physical Journal - Applied Physics, EDP Sciences, 2016, 1286-0042
Other information
Language
English
Type of outcome
Článek v odborném periodiku
Field of Study
10305 Fluids and plasma physics
Country of publisher
France
Confidentiality degree
není předmětem státního či obchodního tajemství
Impact factor
Impact factor: 0.684
RIV identification code
RIV/00216224:14310/16:00088083
Organization unit
Faculty of Science
UT WoS
000380828500016
Keywords in English
Mo2BC coatings; hardness; fracture resistance
Tags
International impact, Reviewed
Změněno: 27/2/2019 10:28, Mgr. Lukáš Zábranský, Ph.D.
Abstract
V originále
Mo2BC thin films show a favourable combination of high stiffness, hardness and elastic modulus together with moderate ductility. In this study we focused on the comparison of mechanical properties of Mo-B-C thin films with different structures (nanocrystalline or amorphous). The thin films were deposited on steel, hard metal and silicon substrates using DC magnetron sputtering. The mechanical properties of Mo-B-C films were studied using indentation techniques under both quasistatic and dynamic conditions using a wide range of loads from 50 mikroN up to 1 N. The results showed that even amorphous Mo-B-C thin films had high hardness of 19.5±0.5 GPa and elastic modulus of 276±5 GPa. Their hardness is comparable with the common amorphous diamond-like carbon coatings. Moreover, their fracture toughness is significantly higher. The results of mechanical tests were correlated with microstructure observations carried out using scanning and transmission electron microscopy. The images of the deformed area under the residual indentation imprints showed no cracking even after high loads or after indentation with sharp cube corner indenter.
Links
ED2.1.00/03.0086, research and development project |
| ||
GA15-17875S, research and development project |
| ||
LO1411, research and development project |
|