PABST, W., E. GREGOROVA, J. KLOUZEK, A. KLOUZKOVA, P. ZEMENOVÁ, M. KOHOUTKOVA, I. SEDLAROVA, K. LANG, M. KOTOUCEK, L. NEVRIVOVA a Dalibor VŠIANSKÝ. High-temperature Young's moduli and dilatation behavior of silica refractories. JOURNAL OF THE EUROPEAN CERAMIC SOCIETY. OXFORD: ELSEVIER SCI LTD, 2016, roč. 36, č. 1, s. 209-220. ISSN 0955-2219. Dostupné z: https://dx.doi.org/10.1016/j.jeurceramsoc.2015.09.020.
Další formáty:   BibTeX LaTeX RIS
Základní údaje
Originální název High-temperature Young's moduli and dilatation behavior of silica refractories
Název česky Vysokoteplotní Youngův modul a dilatace dinasových žáromateriálů
Autoři PABST, W. (203 Česká republika), E. GREGOROVA (203 Česká republika), J. KLOUZEK (203 Česká republika), A. KLOUZKOVA (203 Česká republika), P. ZEMENOVÁ (203 Česká republika), M. KOHOUTKOVA (203 Česká republika), I. SEDLAROVA (203 Česká republika), K. LANG (203 Česká republika), M. KOTOUCEK (203 Česká republika), L. NEVRIVOVA (203 Česká republika) a Dalibor VŠIANSKÝ (203 Česká republika, domácí).
Vydání JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, OXFORD, ELSEVIER SCI LTD, 2016, 0955-2219.
Další údaje
Originální jazyk angličtina
Typ výsledku Článek v odborném periodiku
Obor 20504 Ceramics
Stát vydavatele Velká Británie a Severní Irsko
Utajení není předmětem státního či obchodního tajemství
Impakt faktor Impact factor: 3.454
Kód RIV RIV/00216224:14310/16:00087600
Organizační jednotka Přírodovědecká fakulta
Doi http://dx.doi.org/10.1016/j.jeurceramsoc.2015.09.020
UT WoS 000364254700023
Klíčová slova česky dinas; Youngův modul; elastický modul; dilatace; dilatometrie; cristobalit; tridymit
Klíčová slova anglicky Silica refractories; Young's modulus; Elastic modulus; Dilatation; Dilatometry; Impulse excitation; Cristobalite; Tridymite
Štítky AKR, rivok
Příznaky Mezinárodní význam, Recenzováno
Změnil Změnila: Ing. Andrea Mikešková, učo 137293. Změněno: 6. 4. 2017 18:16.
Anotace
Silica refractories with cristobalite-tridymite ratios between 0.83-0.86 and 1.43-1.47 and porosities of 13-17% are characterized by impulse excitation up to 1200 degrees C and by dilatometry up to 1300 degrees C. During heating, Young's moduli start to decrease from their room temperature values (9-12 GPa) to about 5-7 GPa at 200 degrees C, followed by a very steep increase at around 230 degrees C to values higher than the room temperature values and a nonlinear increase to their final high-temperature values. During cooling, Young's moduli increase even further, exhibit a maximum and a nonlinear decrease that does not follow the heating curve, a very steep decrease at around 200 degrees C and a final increase to the intial room temperature values, so that a closed loop results during thermal cycling. Dilatometric measurements confirm that the strong increase of the Young's modulus at around 230 degrees C (during heating) can be attributed to the phase transition between low- and high-temperature cristobalite, while the more gentle but still very significant changes in Young's moduli below 200 degrees C are due to the more diffuse transitions between tridymite subpolymorphs. Microcracks are identified as the primary cause of the low Young's moduli and their increase with temperature. (C) 2015 Elsevier Ltd. All rights reserved.
Návaznosti
TA02010084, projekt VaVNázev: Vývoj dinasu s optimalizovanými vlastnostmi s důrazem na odolnost proti korozi
Investor: Technologická agentura ČR, Vývoj dinasu s optimalizovanými vlastnostmi s důrazem na odolnost vůči korozi
VytisknoutZobrazeno: 26. 4. 2024 07:19