J 2016

High-temperature Young's moduli and dilatation behavior of silica refractories

PABST, W., E. GREGOROVA, J. KLOUZEK, A. KLOUZKOVA, P. ZEMENOVÁ et. al.

Základní údaje

Originální název

High-temperature Young's moduli and dilatation behavior of silica refractories

Název česky

Vysokoteplotní Youngův modul a dilatace dinasových žáromateriálů

Autoři

PABST, W. (203 Česká republika), E. GREGOROVA (203 Česká republika), J. KLOUZEK (203 Česká republika), A. KLOUZKOVA (203 Česká republika), P. ZEMENOVÁ (203 Česká republika), M. KOHOUTKOVA (203 Česká republika), I. SEDLAROVA (203 Česká republika), K. LANG (203 Česká republika), M. KOTOUCEK (203 Česká republika), L. NEVRIVOVA (203 Česká republika) a Dalibor VŠIANSKÝ (203 Česká republika, domácí)

Vydání

JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, OXFORD, ELSEVIER SCI LTD, 2016, 0955-2219

Další údaje

Jazyk

angličtina

Typ výsledku

Článek v odborném periodiku

Obor

20504 Ceramics

Stát vydavatele

Velká Británie a Severní Irsko

Utajení

není předmětem státního či obchodního tajemství

Impakt faktor

Impact factor: 3.454

Kód RIV

RIV/00216224:14310/16:00087600

Organizační jednotka

Přírodovědecká fakulta

UT WoS

000364254700023

Klíčová slova česky

dinas; Youngův modul; elastický modul; dilatace; dilatometrie; cristobalit; tridymit

Klíčová slova anglicky

Silica refractories; Young's modulus; Elastic modulus; Dilatation; Dilatometry; Impulse excitation; Cristobalite; Tridymite

Štítky

Příznaky

Mezinárodní význam, Recenzováno
Změněno: 6. 4. 2017 18:16, Ing. Andrea Mikešková

Anotace

V originále

Silica refractories with cristobalite-tridymite ratios between 0.83-0.86 and 1.43-1.47 and porosities of 13-17% are characterized by impulse excitation up to 1200 degrees C and by dilatometry up to 1300 degrees C. During heating, Young's moduli start to decrease from their room temperature values (9-12 GPa) to about 5-7 GPa at 200 degrees C, followed by a very steep increase at around 230 degrees C to values higher than the room temperature values and a nonlinear increase to their final high-temperature values. During cooling, Young's moduli increase even further, exhibit a maximum and a nonlinear decrease that does not follow the heating curve, a very steep decrease at around 200 degrees C and a final increase to the intial room temperature values, so that a closed loop results during thermal cycling. Dilatometric measurements confirm that the strong increase of the Young's modulus at around 230 degrees C (during heating) can be attributed to the phase transition between low- and high-temperature cristobalite, while the more gentle but still very significant changes in Young's moduli below 200 degrees C are due to the more diffuse transitions between tridymite subpolymorphs. Microcracks are identified as the primary cause of the low Young's moduli and their increase with temperature. (C) 2015 Elsevier Ltd. All rights reserved.

Návaznosti

TA02010084, projekt VaV
Název: Vývoj dinasu s optimalizovanými vlastnostmi s důrazem na odolnost proti korozi
Investor: Technologická agentura ČR, Vývoj dinasu s optimalizovanými vlastnostmi s důrazem na odolnost vůči korozi