2016
Drinking water contaminants from epoxy resin-coated pipes: A field study
RAJASÄRKKÄ, Suvi Johanna Irene, Marek PERNICA, Jan KUTA, Jonas LASNAK, Zdeněk ŠIMEK et. al.Základní údaje
Originální název
Drinking water contaminants from epoxy resin-coated pipes: A field study
Autoři
RAJASÄRKKÄ, Suvi Johanna Irene (246 Finsko, domácí), Marek PERNICA (203 Česká republika, domácí), Jan KUTA (203 Česká republika, domácí), Jonas LASNAK (203 Česká republika), Zdeněk ŠIMEK (203 Česká republika, domácí) a Luděk BLÁHA (203 Česká republika, garant, domácí)
Vydání
Water Research, OXFORD, PERGAMON-ELSEVIER SCIENCE LTD, 2016, 0043-1354
Další údaje
Jazyk
angličtina
Typ výsledku
Článek v odborném periodiku
Obor
30304 Public and environmental health
Stát vydavatele
Velká Británie a Severní Irsko
Utajení
není předmětem státního či obchodního tajemství
Odkazy
Impakt faktor
Impact factor: 6.942
Kód RIV
RIV/00216224:14310/16:00088670
Organizační jednotka
Přírodovědecká fakulta
UT WoS
000383292100015
Klíčová slova anglicky
Drinking water; Water pipe; Epoxy resin; Spray-on-lining; Bisphenol A
Příznaky
Mezinárodní význam, Recenzováno
Změněno: 5. 4. 2017 09:56, Ing. Andrea Mikešková
Anotace
V originále
Rehabilitation of aged drinking water pipes is an extensive renovation and increasingly topical in many European cities. A commonly used polymer is epoxy resin consisting of monomer bisphenol A (BPA). Leaching of BPA from epoxy lining to drinking water has been a concern among public and authorities. Currently epoxy lining is not recommended in some countries. BPA leaching has been demonstrated in laboratory studies but the behavior and ageing process of epoxy lining in situ is not well known. In this study 6 locations with different age epoxy linings of drinking water pipes done using two distinct technologies were studied. While bisphenol F, 4-nnonylphenol, and 4-t-octylphenol were rarely found and in trace concentrations, BPA was detected in majority of samples. The influence of ageing of epoxy lining on BPA leaching on could be shown in case of LSE technology: locations with 8-9 years old lining leached 4-20-fold more BPA compared to a location with 2-year-old lining. Analysis of metals showed that epoxy lining can reduce especially iron concentration in water. No significant burden to water could be shown by the analyzed 72 volatile organic compounds, including epichlorhydrin, precursor used in epoxy resin. Estrogenicity was detected in water samples with the highest BPA loads. Comparable responses of two yeast bioreporters (estrogen receptor alpha and BPA-targeted) indicated that bisphenol-like compounds were the main cause of estrogenicity. Compared to the estimated average daily BPA exposure, additional BPA load via cold drinking water in the studied locations was low, maximum 8.7%. However, hot water should also be considered as exposure source due to higher BPA concentrations. Epoxy lined locations should be monitored in future in order to evaluate ageing process and control increasing leaching of potentially harmful chemicals.