Fate of Gold Nanoparticles in Laser Desorption/Ionization Mass Spectrometry: Toward the Imaging of Individual Nanoparticles

PRYSIAZHNYI, Vadym, Antonín BEDNAŘÍK, Michal ŽALUD, Veronika HEGROVÁ, Jan NEUMAN et. al.

Základní údaje

Originální název

Fate of Gold Nanoparticles in Laser Desorption/Ionization Mass Spectrometry: Toward the Imaging of Individual Nanoparticles

Autoři

PRYSIAZHNYI, Vadym (203 Česká republika, domácí), Antonín BEDNAŘÍK (203 Česká republika, domácí), Michal ŽALUD (203 Česká republika, domácí), Veronika HEGROVÁ (203 Česká republika), Jan NEUMAN (203 Česká republika) a Jan PREISLER (203 Česká republika, garant, domácí)

Vydání

Journal of the American Society for Mass Spectrometry, American Chemical Society, 2023, 1044-0305

Další údaje

Jazyk

angličtina

Typ výsledku

Článek v odborném periodiku

Obor

10406 Analytical chemistry

Stát vydavatele

Spojené státy

Utajení

není předmětem státního či obchodního tajemství

Odkazy

Impakt faktor

Impact factor: 3.200 v roce 2022

Kód RIV

RIV/00216224:14310/23:00130754

Organizační jednotka

Přírodovědecká fakulta

UT WoS

000953993900001

Klíčová slova anglicky

Gold; Ions; Lasers; Metal nanoparticles; Suspensions

Štítky

Příznaky

Mezinárodní význam, Recenzováno
Změněno: 18. 10. 2024 13:48, Ing. Jana Kuchtová

Anotace

V originále

This study focuses on mapping the spatial distribution of Au nanoparticles (NPs) by laser desorption/ionization mass spectrometry imaging (LDI MSI). Laser interaction with NPs and associated phenomena, such as change of shape, melting, migration, and release of Au ions, are explored at the single particle level. Arrays of dried droplets containing low numbers of spatially segregated NPs were reproducibly prepared by automated drop-on-demand piezo-dispensing and analyzed by LDI MSI using an ultrahigh resolution orbital trapping instrument. To enhance the signal from NPs, an in source gas-phase chemical reaction of generated Au ions with xylene was employed. The developed technique allowed the detecting, chemical characterization, and mapping of the spatial distribution of Au NPs; the ion signals were detected from as low as ten 50 nm Au NPs on a pixel. Furthermore, the Au NP melting dynamics under laser irradiation was monitored by correlative atomic force microscopy (AFM) and scanning electron microscopy (SEM). AFM measurements of Au NPs before and after LDI MSI analysis revealed changes in NP shape from a sphere to a half-ellipsoid and total volume reduction of NPs down to 45% of their initial volume.

Návaznosti

GA21-12262S, projekt VaV
Název: Nanočásticové sondy pro zobrazovací hmotnostní spektrometrii
Investor: Grantová agentura ČR, Nanočásticové sondy pro zobrazovací hmotnostní spektrometrii
MUNI/A/1421/2022, interní kód MU
Název: Vývoj metod a instrumentace pro analýzu biologicky významných látek 2023
Investor: Masarykova univerzita, Vývoj metod a instrumentace pro analýzu biologicky významných látek 2023
90127, velká výzkumná infrastruktura
Název: CIISB II