2020
Adhesive Properties of Silicone-Coated Release Liner Paper Enhanced by Atmospheric Pressure Plasma Pre- and Post-Treatment
KELAR TUČEKOVÁ, Zlata; Oleksandr GALMIZ; Jakub KELAR; Dušan KOVÁČIK; Monika STUPAVSKÁ et al.Základní údaje
Originální název
Adhesive Properties of Silicone-Coated Release Liner Paper Enhanced by Atmospheric Pressure Plasma Pre- and Post-Treatment
Autoři
KELAR TUČEKOVÁ, Zlata; Oleksandr GALMIZ; Jakub KELAR; Dušan KOVÁČIK; Monika STUPAVSKÁ; Petra ŠRÁMKOVÁ; Miroslav ZEMÁNEK; Julien VALLADE a Mirko ČERNÁK
Vydání
Coatings, Basel, MDPI, 2020, 2079-6412
Další údaje
Jazyk
angličtina
Typ výsledku
Článek v odborném periodiku
Obor
10305 Fluids and plasma physics
Stát vydavatele
Švýcarsko
Utajení
není předmětem státního či obchodního tajemství
Odkazy
Impakt faktor
Impact factor: 2.881
Označené pro přenos do RIV
Ano
Kód RIV
RIV/00216224:14310/20:00116978
Organizační jednotka
Přírodovědecká fakulta
UT WoS
EID Scopus
Klíčová slova anglicky
release liner; clay-coated paper; silicone coating; adhesion; wettability changes; aging; plasma treatment; atmospheric pressure plasma
Příznaky
Mezinárodní význam, Recenzováno
Změněno: 27. 2. 2024 15:46, Mgr. Marie Novosadová Šípková, DiS.
Anotace
V originále
For release-liner preparation, coating stabilization of the silicone layer on base paper often requires pre- and post-treatment. In this study, we used atmospheric pressure diffuse coplanar surface barrier discharge in roll-to-roll configuration. The results of prepared coating showed that the A4 size clay-coated paper sprayed with silicone oil (0.25–0.50 mL) gradually decreased the tape peeling force (180°) with prolonged and repeated air plasma post-treatment. Best results showing increased hydrophobicity and significantly enhanced release factor of the coating were obtained after the plasma treatment in a nitrogen atmosphere. The silicone coating on the clay-coated paper reduced the reference release force from 5.5 N/cm to less than 1.5 N/cm after the repeated silicone spraying and short nitrogen plasma post-treatment. The results of X-ray photoelectron spectroscopy and scanning electron microscopy indicate silicone curing by plasma post-treatment and pore-closing of base paper without changes of the bulk material. The aging test lasting 3 months revealed the stability of the prepared coating.