ČOBIČ, Andrea, Vladimir BERMANEC, Nenad TOMAŠIČ a Radek ŠKODA. The hydrothermal recrystallization of metamict allanite-(Ce). Canadian Mineralogist. 2010, roč. 48, č. 3, s. 513-521. ISSN 0008-4476.
Další formáty:   BibTeX LaTeX RIS
Základní údaje
Originální název The hydrothermal recrystallization of metamict allanite-(Ce)
Autoři ČOBIČ, Andrea (191 Chorvatsko), Vladimir BERMANEC (191 Chorvatsko), Nenad TOMAŠIČ (191 Chorvatsko) a Radek ŠKODA (203 Česká republika, garant).
Vydání Canadian Mineralogist, 2010, 0008-4476.
Další údaje
Originální jazyk angličtina
Typ výsledku Článek v odborném periodiku
Obor 10500 1.5. Earth and related environmental sciences
Stát vydavatele Kanada
Utajení není předmětem státního či obchodního tajemství
Impakt faktor Impact factor: 1.289
Kód RIV RIV/00216224:14310/10:00040621
Organizační jednotka Přírodovědecká fakulta
UT WoS 000280414600005
Klíčová slova anglicky allanite-(Ce); metamictization; hydrothermal recrystallization; X-ray diffraction; granitic pegmatite
Příznaky Mezinárodní význam, Recenzováno
Změnil Změnil: doc. Mgr. Radek Škoda, Ph.D., učo 21802. Změněno: 12. 11. 2010 12:09.
Anotace
Samples of metamict allanite-(Ce) originating from granite pegmatites were recrystallized by heating in air and under hydrothermal conditions. Recrystallization in air resulted in partial recovery of the crystal structure at 650oC. Heating at higher temperatures resulted in decomposition of the allanite structure to a multiphase assemblage containing hematite, cerianite, feldspar, britholite and thorianite. To our knowledge, this is the first report of thorianite as a breakdown product of allanite in literature. The collapse of the structure is mainly related to the removal of structural H2O. Recrystallization under hydrothermal conditions yielded a more rapid and complete recovery of the structure at lower temperatures, without the appearance of additional phases. The stability of the allanite structure during hydrothermal recrystallization is related to the retention of OH- groups, available because of the aqueous environment of recrystallization. Also, H2O promotes a more rapid and efficient recrystallization due to the enhanced diffusion of cations. Crystallite size and strain calculation also record evidence of the recovery of the structure of damaged allanite.
Návaznosti
KJB301630801, projekt VaVNázev: Interakce metamiktních minerálů s hydrotermálnímy fluidy a její význam geologickém prostředí
Investor: Akademie věd ČR, Interakce metamiktních minerálů s hydrotermálnímy fluidy a její význam geologickém prostředí
VytisknoutZobrazeno: 31. 7. 2024 16:30