SOBOTA, Jaroslav, Vilma BURSIKOVA, Jan GROSSMAN, Tomas FORT, Petr KLAPETEK, Jiri BURSIK, Daniel FRANTA a Vratislav PERINA. Optimization of the performance of graded amorphous carbon coatings to steel substrates using PECVD. In 2nd conference on New Diamond and Nano Carbons 2008. 2008.
Další formáty:   BibTeX LaTeX RIS
Základní údaje
Originální název Optimization of the performance of graded amorphous carbon coatings to steel substrates using PECVD
Název česky Optimization of the performance of graded amorphous carbon coatings to steel substrates using PECVD
Autoři SOBOTA, Jaroslav, Vilma BURSIKOVA, Jan GROSSMAN, Tomas FORT, Petr KLAPETEK, Jiri BURSIK, Daniel FRANTA a Vratislav PERINA.
Vydání 2nd conference on New Diamond and Nano Carbons 2008, 2008.
Další údaje
Originální jazyk angličtina
Typ výsledku Konferenční abstrakt
Obor 10305 Fluids and plasma physics
Stát vydavatele Tchaj-wan
Utajení není předmětem státního či obchodního tajemství
Organizační jednotka Přírodovědecká fakulta
Klíčová slova anglicky Optimization; performance; graded amorphous carbon coatings; steel substrates; PECVD
Štítky graded amorphous carbon coatings, Optimization, PECVD, performance, steel substrates
Příznaky Mezinárodní význam
Změnil Změnil: Mgr. Adrian Stoica, Ph.D., učo 250983. Změněno: 13. 1. 2009 14:28.
Anotace
For optimization of the performance of the protective coatings there is necessary to optimize the following materials parameters: the elastic modulus, hardness, surface strength, film fracture toughness, impact resistance and film-substrate adhesion. Elastic contact between brittle film and indenting particles may lead to the formation of Hertzian cone cracks. These stresses arise from the radial tensile stresses around the contact area. The resulting strain is difficult to be relaxed and it builds up with increasing film thickness. When the elastic recovery force of the film exceeds a critical value, the stresses in the film are relaxed by cracking or wrinkling resulting in delamination.
Anotace česky
For optimization of the performance of the protective coatings there is necessary to optimize the following materials parameters: the elastic modulus, hardness, surface strength, film fracture toughness, impact resistance and film-substrate adhesion. Elastic contact between brittle film and indenting particles may lead to the formation of Hertzian cone cracks. These stresses arise from the radial tensile stresses around the contact area. The resulting strain is difficult to be relaxed and it builds up with increasing film thickness. When the elastic recovery force of the film exceeds a critical value, the stresses in the film are relaxed by cracking or wrinkling resulting in delamination.
Návaznosti
GA202/07/1669, projekt VaVNázev: Depozice termomechanicky stabilních nanostrukturovaných diamantu-podobných tenkých vrstev ve dvojfrekvenčních kapacitních výbojích
Investor: Grantová agentura ČR, Depozice termomechanicky stabilních nanostrukturovaných diamantu-podobných tenkých vrstev ve dvojfrekvenčních kapacitních výbojích
KAN311610701, projekt VaVNázev: Nanometrologie využívající metod rastrovací sondové mikroskopie
Investor: Akademie věd ČR, Nanometrologie využívající metod rastrovací sondové mikroskopie
VytisknoutZobrazeno: 30. 5. 2024 09:53